2015-02-03; 20:04:05 EST
Member Since
2014-05-06
Posts: 3821
Chuy: Just a few thoughts and suggestions. I used fibreglass on the inside of the join but had to cut the lip off the liner to get in to the area. In my case there was a strip of wood on the inside of the join that was broken and rotted wherever the water reached it so I removed it with a chisel. I also wanted to bond the fibreglass to the deck and hull fibreglass rather than to a weak piece of plywood. Before applying the fibreglass I filled the join area with epoxy thickened with high-strength filler to fill any gaps and old holes and to give a smooth radius for the glass. I used epoxy for everything because of its superior properties but I am sure polyester would work as well. I used two layers of 6" roving tape but plan to add another two layers later because I have no idea how many layers are adequate.. (see pictures). I glassed the joint from the bow to the aft of the cabin at the companionway. I could not see the need to glass the seam beyond that point as a bit of water leaking into the cockpit is not a problem and from what I could see it would be incredibly difficult to get into the area behind the seats to work on the joint. I will probably insert bolts after the fibreglass work is completed but might use rivets. Putting glass over the bolts does not seem like a good idea to me. I would not use 5200 for the bolts as the day may well come when you want to remove them again. Nothing is permanent except the mess that 5200 creates. Using 5200 for the area where the deck and hull overlap might be appropriate but I would be inclined to use the stuff the Rummy used. It is just my bias, but I have never used 5200 when I didn't eventually regret it. If you glass the joint adequately you will need considerably fewer mechanical fasteners so there will be fewer places for leaks to develop. If you also fill the joint with a good sealant I can't see how significant amounts of water could make its way past the rub rail and through the bolt holes. I expect that the leaks were primarily through the joint. In my case the original rivets were aluminium, I think, and there was no rust. If your boat is anything like mine you will not be able to save and reuse the old rub rail. When I replace mine I will use the one-piece flexible vinyl stuff as it looks to be a better product and easier to install. Good luck, Graham Stewart gstewart8 at cogeco.ca 613 389-1737 Hull - Deck join rebuild 2009 (3).jpg Hull - Deck join rebuild 2009 (4).jpg Hull - Deck join rebuild 2009 (6).jpgSee the original archive post